- Product Details
- {{item.text}}
Quick Details
-
Product name:
-
Thermoplastic Elastomer TPE/TPR/TPU Plastic Pellets
-
Material:
-
TPE Material
-
Certificate:
-
/ EN71 /ASTM
-
Appearance:
-
Plastic Granules
-
Style:
-
Raw Material Flame Retardant TPE
-
Hardness:
-
0-100 A
-
Delivery Time:
-
7-15days
-
Density:
-
1.15±0.05
-
Color:
-
Natural or customized
-
Tensile strength:
-
≥5
Quick Details
-
Place of Origin:
-
Jiangsu, China
-
Brand Name:
-
BAIYA
-
Model Number:
-
JL006
-
Product name:
-
Thermoplastic Elastomer TPE/TPR/TPU Plastic Pellets
-
Material:
-
TPE Material
-
Certificate:
-
/ EN71 /ASTM
-
Appearance:
-
Plastic Granules
-
Style:
-
Raw Material Flame Retardant TPE
-
Hardness:
-
0-100 A
-
Delivery Time:
-
7-15days
-
Density:
-
1.15±0.05
-
Color:
-
Natural or customized
-
Tensile strength:
-
≥5
Thermoplastic Elastomer TPE/TPR/TPU Plastic Pellets
Product Description
Commodity | TPE30C | Quality inspection date | 2018/12/13 | |||
No. | Item | Unit | Standard | Determine scope | Testing result | Test method |
1 | Appearance | Visual test | Natural color | Natural color | ||
2 | Hardness | Shore A | ASTM-D2240 | 0~100 | 30C | indoor temperature℃ |
3 | Density | SP.Gr | ASTM-792 | 1.15±0.05 | 1.2 | |
4 | Solution flow index | g/10min | ASTM-D1238 | 5~20 | 13 | 190℃,2.16kg |
5 | Tensile strength | Mpa | ASTM-D412 | ≥5 | 7.8 | indoor temperature 500mm/min |
6 | Elongation | % | ASTM-D412 | ≥500 | 550 | |
7 | Tear strength | KN/m | ASTM-D624 | ≥20 | 23 | |
Manufacturing technique | ||||||
Barrel temperature | Range ℃ | Typical value ℃ | ||||
Forepart | 150-190 | 170 | ||||
Midpiece | 150-210 | 180 | ||||
Back end | 150-210 | 180 | ||||
Orifice/Die-head | 160-200 | 180 | ||||
Upper limit of processing temperature ℃ | 220 | |||||
Time of drying | Generally there is no need to dry,If the storage environment is humid or the production of products surface requirements higher parts,dry in a hot air oven for 2 to 4 hours | |||||
1.The above data is only for reference. The above data can be adjusted according to different models,molds and product requirements.2.Do not allow the material in the barrel to stay too long too long,Please use PE to clean the machine before stopping it. | ||||||