- Product Details
- {{item.text}}
Quick Details
-
Brand Name:
-
Sandite
-
Tensile Stress (100% Strain):
-
2.05 MPa
-
Tensile Stress (300% Strain):
-
5.88 MPa
-
Tensile Strength (Yield):
-
40.0 Mpa
-
Elongation:
-
≥500%
-
Glass Transition Temperature (Tg):
-
<-59.96℃
-
Tear Strength:
-
50.8 kN/m
-
Hardness (Shore A):
-
80
-
Specific Gravity:
-
1.07 g/cm3
-
Color:
-
Transparent
Quick Details
-
color:
-
Transparent
-
Shape:
-
granules
-
Place of Origin:
-
Shandong, China
-
Brand Name:
-
Sandite
-
Tensile Stress (100% Strain):
-
2.05 MPa
-
Tensile Stress (300% Strain):
-
5.88 MPa
-
Tensile Strength (Yield):
-
40.0 Mpa
-
Elongation:
-
≥500%
-
Glass Transition Temperature (Tg):
-
<-59.96℃
-
Tear Strength:
-
50.8 kN/m
-
Hardness (Shore A):
-
80
-
Specific Gravity:
-
1.07 g/cm3
-
Color:
-
Transparent
Product Display



Specification
Tensile Strength ( Yield)
|
40 MPa
|
Elongation
|
≥500%
|
Tear Strength
|
50.8 kN/m
|
Bonding Strength With Inorganic Glass
|
≥22kN/m
|
Hardness ( Shore A)
|
80
|
Glass Transition Temperature (Tg)
|
< -59.96℃
|
Tensile Stress (100% Strain)
|
2.05 Mpa
|
Tensile Stress (300% Strain)
|
5.88 Mpa
|
Related Products

Product Application
Hot Searches