- {{item.text}}
Quick Details
-
MF:
-
/
-
EINECS No.:
-
/
-
Place of Origin:
-
Shandong, China
-
Brand Name:
-
MTL
-
Model Number:
-
rock breaker
-
Application:
-
Chemical additives
-
Appearance:
-
powder
-
Sample:
-
Availiable
-
Shelf life:
-
2 Years
-
Packing:
-
20kg /25kg /bag or 200kg/drum
-
MOQ:
-
500g
-
Storage:
-
Cool Dry Place
-
DELIVERY:
-
Express/air/sea
-
Certification:
-
CE
-
CAS:
-
/
-
Keyword:
-
Rock breaker
-
Color:
-
red Color
Quick Details
-
CAS No.:
-
/
-
Purity:
-
98 / 99
-
Other Names:
-
rock breaker
-
MF:
-
/
-
EINECS No.:
-
/
-
Place of Origin:
-
Shandong, China
-
Brand Name:
-
MTL
-
Model Number:
-
rock breaker
-
Application:
-
Chemical additives
-
Appearance:
-
powder
-
Sample:
-
Availiable
-
Shelf life:
-
2 Years
-
Packing:
-
20kg /25kg /bag or 200kg/drum
-
MOQ:
-
500g
-
Storage:
-
Cool Dry Place
-
DELIVERY:
-
Express/air/sea
-
Certification:
-
CE
-
CAS:
-
/
-
Keyword:
-
Rock breaker
-
Color:
-
red Color
Product Paramenters
Make use of the method and note matters
2, hole distance:
15 to 50cm (the smaller the hole distance, the shorter the cracking time)
3, hole depth:
generally more than 50 cm, too shallow and easy to punch, but not more than 8 meters.
Two, stirring
The ratio of water to medicine is 1:3 (a small package of medicine is about 1.6 kg of water).
In winter, it can be prepared with warm water at 30 to 50 degrees Celsius) to form a liquid slurry. Early morning loading is recommended in summer.
Three, filling holes
1: For vertical straight holes
, the mixed medicine can be directly poured into the hole.
For horizontal or inclined holes, insert a plastic pipe slightly smaller than the aperture of the outer funnel into the hole through the plastic pipe into the hole, while gradually drawing out the plastic pipe, and quickly plug the hole, but there is still no water in the hole cavity.
The whole process including mixing and filling must be completed within 15 minutes (too long time is easy to punch). Install holes in the sequence from outer rows to inner rows.
FOUR. Cracking
Generally cracking within 3 to 10 hours after injection,
if no cracking within 24 hours may be caused by excessive hole distance, should be reduced hole distance, and add holes along the line.
Fifth, the explosive items need to have at least one to two or more free surfaces (free surfaces), so that it can expand the space.
FIVE. Precautions:
1: If the choice of agent is not correct or improper operation, it is possible to punch.
Do not look directly into the hole after loading.
2: Must wear protective glasses to operate, otherwise due to various reasons caused by hole injury incidents have nothing to do with the division.
3: If you are not careful spraying, please clean with plenty of water in time, do not rub, and seek medical attention immediately. The product is alkaline.
|
Application Field: