- Product Details
- {{item.text}}
Quick Details
-
Model Number:
-
n type and p type bismuth telluride
-
Shape:
-
n type round rod/p type square ingot
-
Material:
-
n type doped selenium,p type doped antimony
-
Chemical Composition:
-
99.99% 4n
-
Product Name:
-
n type and p type bismuth telluride ingot
-
Molecular Formula:
-
Bi2Te3, Bite
-
Density at 25 °C(lit.):
-
7.642g.cm-3
-
Color:
-
dark grey
-
CAS No:
-
1304-82-1
-
Melting Point:
-
586℃
-
Doping:
-
N type doped Selenium, P type doped Antimony
-
Seebeck (S):
-
200-230 uV
-
Thermal conductivity (k):
-
1.2-1.6w/m.K
-
Electrical conductivity (rou):
-
850-1250
Quick Details
-
Application:
-
cooling and generating electricity
-
Place of Origin:
-
Hubei, China
-
Brand Name:
-
Tuocai
-
Model Number:
-
n type and p type bismuth telluride
-
Shape:
-
n type round rod/p type square ingot
-
Material:
-
n type doped selenium,p type doped antimony
-
Chemical Composition:
-
99.99% 4n
-
Product Name:
-
n type and p type bismuth telluride ingot
-
Molecular Formula:
-
Bi2Te3, Bite
-
Density at 25 °C(lit.):
-
7.642g.cm-3
-
Color:
-
dark grey
-
CAS No:
-
1304-82-1
-
Melting Point:
-
586℃
-
Doping:
-
N type doped Selenium, P type doped Antimony
-
Seebeck (S):
-
200-230 uV
-
Thermal conductivity (k):
-
1.2-1.6w/m.K
-
Electrical conductivity (rou):
-
850-1250
semiconductors bismuth telluride rods n type and p type bismuth telluride ingot
Product Description
1.Product Description
Characteristics:
|
Bismuth telluride is a compound of tellurium and bismuth. It is a narrow gap layered semiconductor with a trigonal unit cell. It mainly occurs in a rare mineral tellurobismuthite. It's produced by sealing bismuth and tellurium metals in a quartz tube under vacuum.
When alloyed with selenium or antimony, it acts as an efficient thermoelectric material suitable for portable power generation or refrigeration. |
Production Processes:
|
Vacuum melting - crystallization (crystal orientation growth) - regional melting - removal of both ends;
|
Applications:
|
Forming P/N section for semiconductor refrigeration, thermoelectric power generation, etc.
|
2.General Properties
Place of Origin
|
Hubei,China
|
Brand Name
|
Tuocai
|
Material
|
bismuth, tellurium, selenium, antimony
|
Chemical Composition
|
99.99% 4n
|
Molecular formula
|
Bi2Te3, Bite
|
CAS No.
|
1304-82-1
|
Density
|
7.73g/cm3
|
Melting point
|
586℃
|
Surface
|
With Ni & Sn Plated
|
Doping
|
P type bismuth telluride doped Antimony
N type bismuth telluride doped Selenium
|
Seebeck (S)
|
210-230 (alpha, μ V / k) at 300K
|
Electrical conductivity
|
950-1050 (alpha, μ V / k) at 300K
|
Specification
3. Specification
![]() |
Product Model:
|
N-type semiconductor components
|
Production Process:
|
Zone melting crystal pulling process
|
|
Purity:
|
99.99%
|
|
Size:
|
Diameter: 28mm, Length: 190mm-230mm Weight: About 1.2kg/rod |
|
Seebeck coefficient:
|
210-230 (α, μ V / k) at 300K
|
|
Electrical conductivity:
|
950-1050 (α, μ V / k) at 300K
|
![]() |
Product Model:
|
P-type semiconductor components
|
Production Process:
|
Powder metallurgy
|
|
Purity:
|
99.99%
|
|
Size:
|
Dimension: 30x 30x100mm(L*W*H)
Weight: 0.607kg/ingot
|
|
Seebeck coefficient:
|
205-215 (α, μ V / k) at 300K
|
|
Electrical Conductivity:
|
900-1000 (σ, S / cm) at 300K
|
More Products
Bismuth telluride acts as an efficient thermoelectric material for power generation and refrigeration.
Molecular formula is Bi2Te3, it can be processed into Powder, Pellet, Rod, Wafer and other shapes, purity is 99.99%.
Bismuth Telluride Powder: | gneral particle size is 120 mesh,200/325/500/1250mesh are also available. |
Bismuth Telluride Pellet: | gerneral size is 1.4x1.4x1.6mm(L*W*H),other size can be customised. |
Bismuth Telluride Wafer: | size can be produced according to the requirements. |
Bismuth Telluride Rod: | general size of n type round rod is 28mm diameter x 150mm height, p type square rod is 30mm length x 30mm width x 100mm . |
Thermoelectric cooler peltiers are also available.
Hot Searches