Products
Sandeen GL560 Aliphatic urethane-based Glass Lamination Film for marine and rail Glass Ballistic
Sandeen GL560 Aliphatic urethane-based Glass Lamination Film for marine and rail Glass Ballistic
Sandeen GL560 Aliphatic urethane-based Glass Lamination Film for marine and rail Glass Ballistic
Sandeen GL560 Aliphatic urethane-based Glass Lamination Film for marine and rail Glass Ballistic
Sandeen GL560 Aliphatic urethane-based Glass Lamination Film for marine and rail Glass Ballistic
Sandeen GL560 Aliphatic urethane-based Glass Lamination Film for marine and rail Glass Ballistic
Sandeen GL560 Aliphatic urethane-based Glass Lamination Film for marine and rail Glass Ballistic
Sandeen GL560 Aliphatic urethane-based Glass Lamination Film for marine and rail Glass Ballistic

Sandeen GL560 Aliphatic urethane-based Glass Lamination Film for marine and rail Glass Ballistic

FOB Reference Price: Get Latest Price
≥20 Square meters
US $24
Free Inquiry
Customized Request
  • Product Details
  • {{item.text}}

Quick Details

Place of Origin:
Shandong, China
Brand Name:
Sandeen
Tensile Strength:
≥42MPa
Elongation:
≥500%
Tear Strength:
≥40kN/m
Bonding Strength With Inorganic Glass:
≥22kN/m
Hardness:
80~85IRHD
Glass Transition Temperature (Tg):
≤ -68℃
Transmittance:
≥90%
Haze:
≤ 0.3%
Material:
100% TPU

Quick Details

color:
Clear
Shape:
Accept customization
Application:
High-speed train windshield glass, Ship bridge glass, Bulletproof glass for armored vehicles, special purpose vehicle, bulletproof face mask, bulletproof shield, High-speed train windshield glass
Place of Origin:
Shandong, China
Brand Name:
Sandeen
Tensile Strength:
≥42MPa
Elongation:
≥500%
Tear Strength:
≥40kN/m
Bonding Strength With Inorganic Glass:
≥22kN/m
Hardness:
80~85IRHD
Glass Transition Temperature (Tg):
≤ -68℃
Transmittance:
≥90%
Haze:
≤ 0.3%
Material:
100% TPU
Product Describe
Shengding (Qingdao) Advanced Material Co., LTD
Physical Property
Value S.I.Units
Testing Standard
Tensile Strength
≥ 42MPa
GB/T528-2009
Tear Strength
≥ 40kN/m
GB/T529-2008
Bonding Strength with Inorganic Glass
≥ 22kN/m
GJB 446-1988
Glass Transition Temperature (Tg)
≤ - 68℃
GB/T19466.2-2004
Transmittance
≥ 90%
GB/T37831-2019
Hardness
80~85 IRHD
GB/T 531.1-2008
Haze
≤ 0.3%
GB/T37831-2019