- Product Details
- {{item.text}}
Quick Details
-
Voltage:
-
220V/110V
-
Power:
-
2.0A
-
Dimension(L*W*H):
-
16*17*11.5cm
-
Weight (KG):
-
3
-
Application:
-
Gold Chrome Silver Zinc Plating
-
Plating style:
-
Plating
-
Available for:
-
Making Electro Galvanized Wire
Quick Details
-
Place of Origin:
-
Guangdong, China
-
Machine Type:
-
1502 electroplating machine
-
Marketing Type:
-
Hot Product
-
Voltage:
-
220V/110V
-
Power:
-
2.0A
-
Dimension(L*W*H):
-
16*17*11.5cm
-
Weight (KG):
-
3
-
Application:
-
Gold Chrome Silver Zinc Plating
-
Plating style:
-
Plating
-
Available for:
-
Making Electro Galvanized Wire
Products Description
Platinum plating method:
Positive (+): Titanium mesh negative (-): Jewelry
Temperature: 30-40.C
Gold plating time: 90-120 seconds
Note: Electroplating items need to be shaken at the beginning
Technical Parameters:
Maximum adjustable voltage: 20V
Maximum adjustable current: 2.0A
The machine is using voltage: 220V
Gold plating method 14K.18K.24K
Positive (+): Titanium mesh negative (-): Jewelry
Temperature: 70.C-80.C
Gold plating time: 20-50 seconds of electroplating items need to be shaken, from 1 to 4 pieces of ring.
Accessories required for electroplating: beaker, titanium mesh, gold plating machine,
water line, electric furnace, thermometer
Silver plating method:
Positive electrode: Titanium mesh Negative electrode: Clip jewelry, cleaned according to
the electrolytic cleaning salt program, 3 channels after electrolysis
Beaker cleaning, 2.5 g silver salt 54% 500 cc distilled water.
Temperature: 40.c Voltage: 5V Plating time: 3-5 seconds.
Note: All silver salts, electrolytic cleaning salts, and over-beaker cleaning must use
pure distilled water.
Additional information:
1. Polish the light with a cloth wheel and a sander.
2. Then use ultrasonic cleaning machine to add wax water (heating) to clean
3. Polish with a polishing machine
4. Clean with a steam cleaner
5. Finally completed by electrolysis and electroplating procedures
Positive (+): Titanium mesh negative (-): Jewelry
Temperature: 30-40.C
Gold plating time: 90-120 seconds
Note: Electroplating items need to be shaken at the beginning
Technical Parameters:
Maximum adjustable voltage: 20V
Maximum adjustable current: 2.0A
The machine is using voltage: 220V
Gold plating method 14K.18K.24K
Positive (+): Titanium mesh negative (-): Jewelry
Temperature: 70.C-80.C
Gold plating time: 20-50 seconds of electroplating items need to be shaken, from 1 to 4 pieces of ring.
Accessories required for electroplating: beaker, titanium mesh, gold plating machine,
water line, electric furnace, thermometer
Silver plating method:
Positive electrode: Titanium mesh Negative electrode: Clip jewelry, cleaned according to
the electrolytic cleaning salt program, 3 channels after electrolysis
Beaker cleaning, 2.5 g silver salt 54% 500 cc distilled water.
Temperature: 40.c Voltage: 5V Plating time: 3-5 seconds.
Note: All silver salts, electrolytic cleaning salts, and over-beaker cleaning must use
pure distilled water.
Additional information:
1. Polish the light with a cloth wheel and a sander.
2. Then use ultrasonic cleaning machine to add wax water (heating) to clean
3. Polish with a polishing machine
4. Clean with a steam cleaner
5. Finally completed by electrolysis and electroplating procedures
Machine Parameter
Product Name
|
Electroplating machine
|
Platinum plating method
|
Positive (+): Titanium mesh negative (-): Jewelry
Temperature: 30-40.C Gold plating time: 90-120 seconds Note: Electroplating items need to be shaken at the beginning |
Technical Parameters
|
Maximum adjustable voltage: 20V
Maximum adjustable current: 2.0A The machine is using voltage: 220V |
Gold plating method 14K.18K.24K
|
Positive (+): Titanium mesh negative (-): Jewelry
Temperature: 70.C-80.C Gold plating time: 20-50 seconds of electroplating items need to be shaken, from 1 to 4 pieces of ring. Accessories required for electroplating: beaker, titanium mesh, gold plating machine, water line, electric furnace, thermometer |
Silver plating method
|
Positive electrode: Titanium mesh Negative electrode: Clip jewelry, cleaned according to
the electrolytic cleaning salt program, 3 channels after electrolysis Beaker cleaning, 2.5 g silver salt 54% 500 cc distilled water. Temperature: 40.c Voltage: 5V Plating time: 3-5 seconds. Note: All silver salts, electrolytic cleaning salts, and over-beaker cleaning must use pure distilled water. |
Additional information
|
1. Polish the light with a cloth wheel and a sander.
2. Then use ultrasonic cleaning machine to add wax water (heating) to clean 3. Polish with a polishing machine 4. Clean with a steam cleaner 5. Finally completed by electrolysis and electroplating procedures |
Packaging
|
15V2A plating machine * 1
Titanium mesh * 1 Waterline * 1 Alligator clip * 2 |
Customized logo
|
support
|
sample
|
support
|
Packing & Delivery
Packing:
Machine packing inside is plastic films and outside is fumigation wooden case.
Our wooden case is very strong,it can bear long time shipping on the sea.
And machine with preservative film, it can stop the salt sea water enter into the machine and make the machine corrosion.
Our wooden case is very strong,it can bear long time shipping on the sea.
And machine with preservative film, it can stop the salt sea water enter into the machine and make the machine corrosion.
Delivery:
For machines are big and heavy parcel, and different country with different delivery cost,so we suggest below delivery solution:
1. Over 1CBM or 100KG, we suggest send by Sea.
2. Below 1CBM or 100KG, we suggest send by Air.
3. Below 0.5CBM or 50KG, we suggest send by Express.
The price show on our website just the machine EXW price, please contact us for confirm delivery cost before you place order.
1. Over 1CBM or 100KG, we suggest send by Sea.
2. Below 1CBM or 100KG, we suggest send by Air.
3. Below 0.5CBM or 50KG, we suggest send by Express.
The price show on our website just the machine EXW price, please contact us for confirm delivery cost before you place order.
Hot Searches